Nickel-chrome base alloy for ceramic, beryllium free
- Excellent adhesion to ceramic.
- For use with American and European ceramics.
- Content : Ni. 65.50 % - Cr. 19.00 % - Mo. 8.00 %
- T.E.C. :15.3 x 10-6 ºK -1
- Melting range : 1338 - 1347 ºC
- Vickers hardness : 340
|
In a study done in 1989 on metallic ion liberation |
PACKAGING: 250 g JAR.